Seismic Certified™ products are tested to meet the new AWS 'D' designator requirements, making them excellent welding options for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.
To find typical and actual certificates for products use the table below. Once you find the products you are looking for, click the pdf icon to download.
| Wire | AWS Classification | Download |
|---|---|---|
| Coreshield 6 | AWS 5.20; E70T-6D | |
| Coreshield 8 | AWS A5.20; E71T-8D | |
| Dual Shield 710X | AWS A5.20; E71T-1CD/T-9CD | |
| Dual Shield 7100 LC | AWS A5.20; E71T-1CDH8/T-9CDH8 | |
| Dual Shield 7100 Ultra | AWS A5.20; E71T-1MD/T-9MD | |
| Dual Shield 7100 Ultra | AWS A5.20; E71T-1CDH8/T-9CDH8 | |
| Dual Shield II 80-Ni1H4 | AWS A5.29; E81T1-Ni1MJDH4 | |
| Dual Shield II 81-K2 | AWS A5.29; E81T1-K2MD | |
| Dual Shield II 81-K2 | AWS A5.29; E81T1-K2CD | |
| Dual Shield R-70 Ultra 1/16" | AWS A5.20; E70T-1CDH8/T-9CDH8 | |
| Dual Shield R-70 Ultra 3/32" | AWS A5.20; E70T-1CDH8/T-9CDH8 |